Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-7968 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Dynamic stressed parts.Isotrop.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-8064 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-8070 VP Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Processing Temperature | <= 290 °C | <= 554 °F | |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1/AR/5/NT Polyamide 66, with aramid reinforcement Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Isotropic shrinkage characteristics.Control disks, cams, s.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1/XCF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-7139-1 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/BK Polyamide 66, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Processing Temperature | 290 °C | 554 °F | |
Shinil Chemical SHINCON PES-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Processing Temperature | 290 °C | 554 °F | Injection, recommended |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Processing Temperature | <= 290 °C | <= 554 °F | |
Addcomp ADD-VANCE® UV 50 20% active PE based anti-UV masterbatch Fields of application: Foils, films, fibers, extruded and injection molded articles made from PE compatible resins.Examples: Tapes, ropes, carpets, non-wovens, films, fibers, garden furniture, autom.. |
|||
Processing Temperature | 290 °C | 554 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Comtuf® 633 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Processing Temperature | 290 °C | 554 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Comtuf® 635 Nylon 6/6, Glass/Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has .. |
|||
Processing Temperature | 290 °C | 554 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Lubrilon® 604 Nylon 6/6, PTFE/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Processing Temperature | 290 °C | 554 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Lubrilon® 605 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Processing Temperature | 290 °C | 554 °F | Injection, recommended |
Arkema Group Rilsan® Clear G350 Polyamide Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor.. |
|||
Processing Temperature | 290 °C | 554 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Lubrilon® 631 Nylon 6/6, Graphite/Molybdenum Disulfide Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Processing Temperature | 290 °C | 554 °F | See Materials Notes |
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Dry)
(discontinued **) Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend.. |
|||
Processing Temperature | 290 °C | 554 °F | mass temp |
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |