Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 188 °C | 370 °F | Recommended Stock Extrusion |
S&E Specialty Polymers TufTech™ GA-5748C-01 PVC Compound Application: RoHS compliant, PVC based compound suitable for THHN, THWN, applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
Processing Temperature | 188 - 227 °C | 370 - 440 °F | Average value: 204 °C Grade Count:3 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Processing Temperature | 188 - 216 °C | 370 - 421 °F | |
Shuman 502 Black Polypropylene Copolymer Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Processing Temperature | 188 - 216 °C | 370 - 421 °F | |
Shuman 502C Black Polypropylene Copolymer Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Processing Temperature | 188 - 216 °C | 370 - 421 °F | |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |
|||
Processing Temperature | 188 - 227 °C | 370 - 440 °F | Blow Molding Stock Temp. |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding Stock Temp. |
Total HDPE MS201 BN-NA High Density Polyethylene - Fuel Tank Resin Polyethylene: High molecular weight, high density fuel tank resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceGMP.PE.062 certification.Appl.. |
|||
Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 188 °C | 370 °F | Film extrusion temperature |
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21.. |
|||
Processing Temperature | 188 °C | 370 °F | Film extrusion temperature |
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl.. |
|||
Processing Temperature | 188 °C | 370 °F | Film extrusion temperature |
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade DOW LDPE 607A resin is a fully formulated high clarity blown film resin for thin gauge optical applications, such as bakery film. It contains medium levels of slip additive and low levels of antiblo.. |
|||
Processing Temperature | 188 - 227 °C | 370 - 440 °F | Average value: 209 °C Grade Count:8 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |