Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow LDPE 530A Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 530A Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
Thickness 40.0 microns
1.57 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg
2.0 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.8 MPa
1710 psi
Film Tensile Strength at Yield, TD 11.6 MPa
1680 psi
Film Elongation at Break, MD 300 %
300 %
Film Elongation at Break, TD 600 %
600 %
Coefficient of Friction 0.50
0.50
Elmendorf Tear Strength MD 300 g
300 g
Elmendorf Tear Strength TD 170 g
170 g
Elmendorf Tear Strength, MD 7.50 g/micron
191 g/mil
Elmendorf Tear Strength, TD 4.30 g/micron
109 g/mil
Dart Drop 2.80 g/micron
71.1 g/mil
Film Tensile Strength at Break, MD 25.7 MPa
3730 psi
Film Tensile Strength at Break, TD 22.2 MPa
3220 psi
Optical Properties Metric English Comments
Haze 5.4 %
5.4 %
Gloss 67 %
67 %
45°
Processing Properties Metric English Comments
Processing Temperature 188 °C
370 °F
Film extrusion temperature