Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 - 260 °C | 351 - 500 °F | Profile temperatures |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Processing Temperature | 177 - 260 °C | 351 - 500 °F | Profile temperatures |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **) A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer designed for glazing and sealing applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonat.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Vyram™ 9271-85 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | Optimum Tunnel temperature range. |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Processing Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 177 - 191 °C | 350 - 375 °F | Recommended Stock Temperature |
Sylvin Technologies 5748 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo Gem-Tone GC-19F Sapphire Blue Gem-Tone™ Sapphire Blue is a rich blue colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of this colorant. N.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-11 Aurora Pink DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-12 Neon Red DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-14 Fire Orange DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-17 Saturn Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-18 Signal Green DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | 177 °C | 350 °F | Optimum cure is 2 hr. @ 350°F |
Armstrong A-706 Epoxy Adhesive A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent m.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2165 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Processing Temperature | 177 °C | 351 °F | |
Advanced Polymer Alloys Alcryn® 2170 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 3055 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 198 °C Grade Count:17 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Recommended Stock Temperature |
Sylvin Technologies 6055 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |