Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Processing Temperature | 160 - 200 °C | 320 - 392 °F | Extrusion cylinder temperature |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Blow molding |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Flat-sheet |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | Coatings |
Lucobit Lucofin® 1413 Polyolefin TPO Granules, Dark Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucofin® 1454 Polyolefin TPO Granules, Green Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucolit® 1321 Polyolefin TPO Granules, Blue Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucolit® 1322 Polyolefin TPO Granules, Red Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | |
Taiwan Sheen Soon Sheenthane® A7090 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | |
Taiwan Sheen Soon Sheenthane® A8631N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 °C | 320 °F | Hot Forming Temperature |
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Extrusion |
Dyna-Purge® X Purging Compound Designed for Sheet & Profile ExtrusionGeneral Description:DYNA-PURGE X is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to have a natural flow throug.. |
|||
Processing Temperature | 160 - 220 °C | 320 - 428 °F | |
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grindin.. |
|||
Processing Temperature | 160 °C | 320 °F | Cure Measuring Temperature |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |
|||
Processing Temperature | 160 - 220 °C | 320 - 428 °F | Extrusion |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Processing Temperature | 160 - 220 °C | 320 - 428 °F | Extrusion |
BASF Elastollan C 65 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |