Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific)
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific)
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East)
Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm.
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
37.2 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific)
Transparent Polycarbonate in natural color. Excellent processability, super high flow.
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® 545 BK504 PET  (Unverified Data**)
Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont..
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..