Polymer Property : CTE, linear, Parallel to Flow = 9.44 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 100 - 200 °C
9.44 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 0.000 - 100 °C
9.44 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 100 - 200 °C
9.44 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 0.000 - 100 °C
9.44 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK
LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific)
LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber.
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific)
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 100 - 200 °C
9.44 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)  (discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00CES PA 66
LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific)
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RX06424 PA 66
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 100 - 200 °C
9.44 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 0.000 - 100 °C
9.44 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 100 - 200 °C
9.44 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..