Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® AD143 PC LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® IFX6420Z PC (Asia Pacific) Lexan* IFX6420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics Lexan® LSHF PC Clear PolyCarbonate, High Flow, UV Stabilization, Heat StabilizationThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Asia Pacific) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics PC0700 PC PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics PC2203R PC (Europe-Africa-Middle East) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |