Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific) LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific. |