Polymer Property : CTE, linear, Parallel to Flow = 63.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature 0.000 - 32.0 °C
35.0 µin/in-°F

@Temperature 32.0 - 89.6 °F
ASTM E831
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12)
Information provided by PolyOne
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific)
Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC
LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX04462C PC
LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX04490 PC
LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
35.0 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
35.0 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT
LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT
LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific)
LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific)
LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC (Asia Pacific)
LNP* Stat-kon* DEL339XF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant,..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific)
LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
35.0 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature 180 °C
35.0 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® P 3010 MR SW 10101 PPSU
Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati..
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS
LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific.
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific)
LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.