Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 59.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature 180 °C
32.8 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature 180 °C
32.8 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature 140 - 180 °C
32.8 µin/in-°F

@Temperature 284 - 356 °F
ISO 11359-1/-2
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature 180 °C
32.8 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
CTE, linear, Parallel to Flow 59.0 µm/m-°C

@Temperature 180 °C
32.8 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® E 2010 SW Q31 10088 PESU
Information provided by BASF
Copyright © lookpolymers.com All Rights Reserved