Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature 60.0 - 138 °C |
16.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 780 PBT 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature 60.0 - 138 °C |
16.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific) LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 28.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |