Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |