Thermal Properties Metric English Comments
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, weld metal as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Solidus 1300 °C
2370 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Solidus 1300 °C
2370 °F
Special Metals MONEL® Alloy 400
A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem..
Solidus 1300 °C
2370 °F
Special Metals MONEL® Alloy R-405
The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a..
Solidus 1300 °C
2370 °F
Special Metals NIMONIC® Alloy 263
A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an..
Solidus 1300 °C
2370 °F
Special Metals NIMONIC® Alloy PK33
A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h..
Solidus 1300 °C
2370 °F
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Solidus 1300 °C
2370 °F
Goodfellow Nickel 70/Copper 30 Alloy
Information provided by Goodfellow.
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Solidus 1300 °C
2370 °F
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Solidus 1300 °C
2370 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium ..