| Category | Metal , Nonferrous Metal , Nickel Alloy , Superalloy |
| Manufacturer | Haynes International, Inc. |
| Trade Name | Hastelloy® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.86 g/cc | 0.320 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 794 MPa | 115000 psi | |
| 234 MPa @Temperature 927 °C |
33900 psi @Temperature 1700 °F |
||
| 385 MPa @Temperature 815 °C |
55800 psi @Temperature 1500 °F |
||
| 480 MPa @Temperature 704 °C |
69600 psi @Temperature 1300 °F |
||
| 599 MPa @Temperature 593 °C |
86900 psi @Temperature 1100 °F |
||
| Tensile Strength, Yield | 314 MPa @Strain 0.200 % |
45500 psi @Strain 0.200 % |
|
| 179 MPa @Strain 0.200 %, Temperature 927 °C |
26000 psi @Strain 0.200 %, Temperature 1700 °F |
||
| 203 MPa @Strain 0.200 %, Temperature 815 °C |
29400 psi @Strain 0.200 %, Temperature 1500 °F |
||
| 218 MPa @Strain 0.200 %, Temperature 704 °C |
31600 psi @Strain 0.200 %, Temperature 1300 °F |
||
| 227 MPa @Strain 0.200 %, Temperature 593 °C |
32900 psi @Strain 0.200 %, Temperature 1100 °F |
||
| Elongation at Break | 50.7 % | 50.7 % | in 50.8 mm |
| 24.3 % @Temperature 815 °C |
24.3 % @Temperature 1500 °F |
in 50.8 mm | |
| 30 % @Temperature 927 °C |
30 % @Temperature 1700 °F |
in 50.8 mm | |
| 30 % @Temperature 704 °C |
30 % @Temperature 1300 °F |
in 50.8 mm | |
| 45.3 % @Temperature 593 °C |
45.3 % @Temperature 1100 °F |
in 50.8 mm | |
| Modulus of Elasticity | 122 GPa @Temperature 1049 °C |
17700 ksi @Temperature 1920 °F |
|
| 136 GPa @Temperature 1000 °C |
19700 ksi @Temperature 1830 °F |
||
| 143 GPa @Temperature 954 °C |
20700 ksi @Temperature 1750 °F |
||
| 151 GPa @Temperature 904 °C |
21900 ksi @Temperature 1660 °F |
||
| 157 GPa @Temperature 854 °C |
22800 ksi @Temperature 1570 °F |
||
| 163 GPa @Temperature 800 °C |
23600 ksi @Temperature 1470 °F |
||
| 171 GPa @Temperature 700 °C |
24800 ksi @Temperature 1290 °F |
||
| 181 GPa @Temperature 577 °C |
26300 ksi @Temperature 1070 °F |
||
| 181 GPa @Temperature 632 °C |
26300 ksi @Temperature 1170 °F |
||
| 187 GPa @Temperature 500 °C |
27100 ksi @Temperature 932 °F |
||
| 192 GPa @Temperature 410 °C |
27800 ksi @Temperature 770 °F |
||
| 202 GPa @Temperature 221 °C |
29300 ksi @Temperature 430 °F |
||
| 219 GPa @Temperature 14.0 °C |
31800 ksi @Temperature 57.2 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 12.3 µm/m-°C @Temperature 21.0 - 316 °C |
6.83 µin/in-°F @Temperature 69.8 - 601 °F |
|
| 12.7 µm/m-°C @Temperature 21.0 - 427 °C |
7.06 µin/in-°F @Temperature 69.8 - 801 °F |
||
| 13.4 µm/m-°C @Temperature 21.0 - 538 °C |
7.44 µin/in-°F @Temperature 69.8 - 1000 °F |
||
| 14.0 µm/m-°C @Temperature 21.0 - 649 °C |
7.78 µin/in-°F @Temperature 69.8 - 1200 °F |
||
| 14.7 µm/m-°C @Temperature 21.0 - 760 °C |
8.17 µin/in-°F @Temperature 69.8 - 1400 °F |
||
| 15.3 µm/m-°C @Temperature 21.0 - 871 °C |
8.50 µin/in-°F @Temperature 69.8 - 1600 °F |
||
| 15.8 µm/m-°C @Temperature 21.0 - 982 °C |
8.78 µin/in-°F @Temperature 69.8 - 1800 °F |
||
| Specific Heat Capacity | 0.419 J/g-°C @Temperature 100 °C |
0.100 BTU/lb-°F @Temperature 212 °F |
|
| 0.440 J/g-°C @Temperature 200 °C |
0.105 BTU/lb-°F @Temperature 392 °F |
||
| 0.456 J/g-°C @Temperature 300 °C |
0.109 BTU/lb-°F @Temperature 572 °F |
||
| 0.469 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
||
| 0.477 J/g-°C @Temperature 480 °C |
0.114 BTU/lb-°F @Temperature 896 °F |
||
| 0.485 J/g-°C @Temperature 540 °C |
0.116 BTU/lb-°F @Temperature 1000 °F |
||
| 0.523 J/g-°C @Temperature 570 °C |
0.125 BTU/lb-°F @Temperature 1060 °F |
||
| 0.565 J/g-°C @Temperature 590 °C |
0.135 BTU/lb-°F @Temperature 1090 °F |
||
| 0.578 J/g-°C @Temperature 680 °C |
0.138 BTU/lb-°F @Temperature 1260 °F |
||
| 0.578 J/g-°C @Temperature 700 °C |
0.138 BTU/lb-°F @Temperature 1290 °F |
||
| 0.582 J/g-°C @Temperature 660 °C |
0.139 BTU/lb-°F @Temperature 1220 °F |
||
| 0.586 J/g-°C @Temperature 620 °C |
0.140 BTU/lb-°F @Temperature 1150 °F |
||
| Thermal Conductivity | 11.5 W/m-K | 79.8 BTU-in/hr-ft²-°F | RT |
| 13.1 W/m-K @Temperature 100 °C |
90.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
||
| 13.1 W/m-K @Temperature 200 °C |
90.9 BTU-in/hr-ft²-°F @Temperature 392 °F |
||
| 14.4 W/m-K @Temperature 300 °C |
99.9 BTU-in/hr-ft²-°F @Temperature 572 °F |
||
| 16.5 W/m-K @Temperature 400 °C |
115 BTU-in/hr-ft²-°F @Temperature 752 °F |
||
| 18.0 W/m-K @Temperature 500 °C |
125 BTU-in/hr-ft²-°F @Temperature 932 °F |
||
| 20.3 W/m-K @Temperature 600 °C |
141 BTU-in/hr-ft²-°F @Temperature 1110 °F |
||
| 23.6 W/m-K @Temperature 700 °C |
164 BTU-in/hr-ft²-°F @Temperature 1290 °F |
||
| Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
| Solidus | 1300 °C | 2370 °F | |
| Liquidus | 1400 °C | 2550 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al + Ti | <= 0.50 % | <= 0.50 % | |
| Carbon, C | <= 0.080 % | <= 0.080 % | |
| Chromium, Cr | 7.0 % | 7.0 % | |
| Cobalt, Co | <= 0.20 % | <= 0.20 % | |
| Copper, Cu | <= 0.35 % | <= 0.35 % | |
| Iron, Fe | <= 5.0 % | <= 5.0 % | |
| Manganese, Mn | <= 0.80 % | <= 0.80 % | |
| Molybdenum, Mo | 16 % | 16 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | RT |
| 0.000124 ohm-cm @Temperature 815 °C |
0.000124 ohm-cm @Temperature 1500 °F |
||
| 0.000126 ohm-cm @Temperature 705 °C |
0.000126 ohm-cm @Temperature 1300 °F |