Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.50 W/m-K @Temperature 1100 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 46 S Dense Refractory Brick Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05%.. |
|||
Thermal Conductivity | 1.50 W/m-K @Temperature 1100 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 50 Dense Refractory Brick Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato.. |
|||
Thermal Conductivity | 1.50 - 1.60 W/m-K @Temperature 1400 °C |
10.4 - 11.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Thermal Conductivity | 1.50 - 1.60 W/m-K @Temperature 1400 °C |
10.4 - 11.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Thermal Conductivity | 1.50 - 1.70 W/m-K @Temperature 1400 °C |
10.4 - 11.8 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Thermal Conductivity | 1.50 - 1.70 W/m-K @Temperature 1400 °C |
10.4 - 11.8 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Thermal Conductivity | 1.50 W/m-K @Temperature 23.0 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Kuraray Vectran® HT 1500/300 LCP Fiber  is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an.. |
|||
Thermal Conductivity | 1.50 - 1.60 W/m-K @Temperature 1400 °C |
10.4 - 11.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Thermal Conductivity | 1.50 - 1.70 W/m-K @Temperature 1400 °C |
10.4 - 11.8 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Thermal Conductivity | 1.50 W/m-K @Temperature 50.0 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 122 °F |
(Apparent), Product Property; ASTM D5470 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |