Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 87.0 °C @Load 5.001 kg |
189 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 87.0 °C @Load 5.001 kg |
189 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC B8075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 87.0 °C @Load 5.10 kg |
189 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Vicat Softening Point | 87.0 °C @Load 5.10 kg |
189 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 6080 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Vicat Softening Point | 87.0 °C @Load 5.10 kg |
189 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Vicat Softening Point | 87.0 °C @Load 5.00 kg |
189 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 0810 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, high impact resistance, good melt flow rate, good light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 87.0 °C @Load 5.00 kg |
189 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polyrex® PH-55Y Polystyrene - Food Medium impact |
|||
Vicat Softening Point | 87.0 °C @Load 5.00 kg |
189 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Vicat Softening Point | 87.0 °C @Load 5.00 kg |
189 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |