Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C

@Load 5.001 kg
189 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 87.0 °C

@Load 5.001 kg
189 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC B8075 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 87.0 °C

@Load 5.10 kg
189 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPH 11012 Polypropylene Homopolymer, Injection Molding
Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed ..
Vicat Softening Point 87.0 °C

@Load 5.10 kg
189 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPH 6080 Polypropylene Homopolymer, Cast Film
Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH..
Vicat Softening Point 87.0 °C

@Load 5.10 kg
189 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPH 6088 Polypropylene Homopolymer, Cast Film
Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH..
Vicat Softening Point 87.0 °C

@Load 5.00 kg
189 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 0810 V0 Flame Retardant Polystyrene
Flame retardant class V0, PBDE free, high impact resistance, good melt flow rate, good light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 87.0 °C

@Load 5.00 kg
189 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-55Y Polystyrene - Food
Medium impact
Vicat Softening Point 87.0 °C

@Load 5.00 kg
189 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
High impact
Vicat Softening Point 87.0 °C

@Load 5.00 kg
189 °F

@Load 11.0 lb
120°C/hr; ISO 306