Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 130 °C @Load 1.00 kg |
266 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYelast TPE HJ753 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 130 °C @Load 5.001 kg |
266 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF15030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 130 °C @Load 5.001 kg |
266 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS7 F20 PBT/ASA Blend, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 130 °C @Load 1.00 kg |
266 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 130 °C @Load 1.00 kg |
266 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP HJ752 UV Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EE260AI Polypropylene TPO Compound Daplen™ EE260AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Vicat Softening Point | 130 °C @Load 5.10 kg |
266 °F @Load 11.2 lb |
ISO 306 |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 10232 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10232 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 12222 Random Copolymer Polypropylene Total Petrochemicals PPR 12222 is a high melt flow index, clarified random copolymer. Its high transparency makes it particularly suitable for the production of household articles and packaging. It.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 12232 Random Copolymer Polypropylene Total Petrochemicals PPR 12232 is a high melt flow index, high transparency random copolymer. Its has an excellent food compatibility due to its low odor, making it especially suitable for the produ.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion Polypropylene PPR 3221 is a high clarity, high impact resistance random copolymer especially designed for blow molding applications (mono and multi-layers) for food and non-food packaging of sauces,.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 7227 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 7227 is a high transparency random copolymer polypropylene specially developed for the injection molding of caps and closures and articles with high transparency, excellent .. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |
|||
Vicat Softening Point | 130 °C @Load 5.00 kg |
266 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 0820 GF Polycarbonate ABS Blend, 10% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 10% glass fiber reinforcementGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 130 °C @Load 5.00 kg |
266 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 8500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
Vicat Softening Point | 130 °C @Load 0.999 kg |
266 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0815 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 130 °C @Load 5.10 kg |
266 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® T80 XG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt.. |
|||
Vicat Softening Point | 130 °C @Load 5.10 kg |
266 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® T85 SG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig.. |
|||
Vicat Softening Point | >= 130 °C @Load 0.999 kg |
>= 266 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Vicat Softening Point | 130 °C @Load 0.999 kg |
266 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Vicat Softening Point | >= 130 °C @Load 5.00 kg |
>= 266 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Vicat Softening Point | 130 °C @Load 5.00 kg |
266 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Vicat Softening Point | 130 °C @Load 1.02 kg |
266 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals. |