Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS7 FR UV PC/ASA Blend, Flame-Retardant, UV Stabilized Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C @Load 0.999 kg |
248 °F @Load 2.20 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, chlorine and bromine free, excellent light resistance, high impact resistance, excellent processabilityInformation pro.. |
|||
Vicat Softening Point | 120 °C @Load 0.999 kg |
248 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1020 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® T65 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding, easy .. |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Vicat Softening Point | >= 120 °C @Load 5.00 kg |
>= 248 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Vicat Softening Point | 120 °C @Load 5.00 kg |
248 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |