Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 500 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 - 260 °C
239 - 500 °F
Average value: 249 °C Grade Count:20
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Maximum Service Temperature, Air 220 - 260 °C
428 - 500 °F
Average value: 248 °C Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Maximum Service Temperature, Air 250 - 260 °C
482 - 500 °F
Average value: 257 °C Grade Count:7
Overview of materials for Polyamide-Imide, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp..
Maximum Service Temperature, Air 250 - 260 °C
482 - 500 °F
Average value: 258 °C Grade Count:4
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Maximum Service Temperature, Air 25.0 - 260 °C
77.0 - 500 °F
Average value: 136 °C Grade Count:61
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Maximum Service Temperature, Air 250 - 260 °C
482 - 500 °F
Zeus PEEK Tubing
PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used..
Maximum Service Temperature, Air 250 - 260 °C
482 - 500 °F
Average value: 257 °C Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Maximum Service Temperature, Air 200 - 260 °C
392 - 500 °F
Average value: 227 °C Grade Count:9
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Maximum Service Temperature, Air 180 - 260 °C
356 - 500 °F
Average value: 215 °C Grade Count:25
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Copyright © lookpolymers.com All Rights Reserved