Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 230 °C | 446 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica PEEK Polyetheretherketone Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance w.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | short term |
Lehmann & Voss LUVOCOM® 2607-7921 Blend based on polyaryl ether ketone, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Freudenberg Simrit SC1210 S310 Silicone Elastomer Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and b.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM Fluoraz® 888 polytetrafluoroethylene/propylene (FEPM) performs well in aggressive chemicals where ultra pure materials are not required. Recommended for conventional wet and dry system applicatio.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Isoflon Tisoflon® 6K Polytetrafluoroethylene Coated Kevlar Fabric PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Möller Medical NanoSkin 90 NanoCoating Boiling-water resistant, non-abrasive, dirt-repellant, biocompatible coating with very good chemical resistance.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | ASTM D1329 |
Seals Eastern Perflas® 9294 Perfluorinated Rubber Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good .. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | Short peaks operation |
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber 15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | Short peaks operation |
Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber 33% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Trelleborg Emerson & Cuming Eccobond® 104 Two-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 104 Eccobond® Two-Component High Temperature Performance Epoxy AdhesiveFilled, heat curing, high temperature resistant, epoxy adhesive. Excellent chemical resistance. Maintains hig.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | |
Dow Corning 735 OIL RESISTANT SEALANT Black RTV that resists most oils, coolants, etc.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
EMS-Grivory Grivory® TSG-30/4 PA666-GF30 Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | Long Term |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | Long Term |
Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation Information provided by Brandenburger Isoliertechnik GmbH&Co. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
Adamas Adalon® 401 PTFE, 10% Polyimide Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
Adamas Adalon® 415 PTFE, 10% Organic Filler Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
Adamas Adalon® 436 PTFE, 15% Ekonol® Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
Adamas Adalon® 466 PTFE, Mineral/Organic Filler Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
Adamas Adalon® 451 PTFE, organic filler Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | UL temperature Index 220/240°C (430/460°F) |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | < 50 hours; IEC 60216-P1 |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | < 50 hours; IEC 60216-P1 |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |
|||
Maximum Service Temperature, Air | 230 °C | 446 °F | UL-746 B |
Saint-Gobain Norton® MFA Fluoropolymer Film Features/Benefits:Outstanding clarityPerformance from -254°C (-425°F) to 230°C (446°F)Outstanding flex life and stress-crack resistanceOutstanding anti-stick release propertiesExcellent electric.. |