Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1750 °C
3180 °F
no load
McDanel Advanced Ceramics AP 35 99% Alumina
Information provided by McDanel Advanced Ceramic Technologies
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AC 80-5 Dense Refractory Brick
Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from..
Maximum Service Temperature, Air 1750 °C
3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 90 Dense Refractory Brick
Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine..
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 99 S Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu..
Maximum Service Temperature, Air 1750 °C
3180 °F
Gouda Vuurvast CURAS PBK D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This moldable contains a phosphate binding agent and has a low silica cont..
Maximum Service Temperature, Air 1750 °C
3180 °F
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material
Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo..
Maximum Service Temperature, Air 1750 °C
3180 °F
ICE Al2O3 96
Data provided by the manufacturer, International Ceramic Engineering.
Maximum Service Temperature, Air 1750 °C
3180 °F
ICE Al2O3 99.5
Data provided by the manufacturer, International Ceramic Engineering.
Maximum Service Temperature, Air 1750 °C
3180 °F
ICE Al2O3 99.8
Data provided by the manufacturer, International Ceramic Engineering.
Maximum Service Temperature, Air 1750 °C
3180 °F
Gouda Vuurvast AK 85 KM Dense Refractory Brick
Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a..
Maximum Service Temperature, Air 1750 °C
3180 °F
Gouda Vuurvast AK 85 KP Dense Refractory Brick
Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data r..
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 99 Dense Refractory Brick
Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T..
Maximum Service Temperature, Air 1750 °C
3180 °F
Gouda Vuurvast CURAS PBK Moldable Refractory Material
Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at..
Maximum Service Temperature, Air 1750 °C
3180 °F
Sharadaa Ceramics PHOSTCAST 90 XL Phosphate Bonded Castables
Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and ..
Maximum Service Temperature, Air 1750 °C
3180 °F
Sharadaa Ceramics REFCAST A High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Maximum Service Temperature, Air 1750 °C
3180 °F
Sharadaa Ceramics REFCAST LC90ABR Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Maximum Service Temperature, Air 1750 °C
3180 °F
No Load
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Maximum Service Temperature, Air 1750 °C
3180 °F
No Load
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Maximum Service Temperature, Air 1750 °C
3180 °F
No Load
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Maximum Service Temperature, Air 1750 °C
3180 °F
NO-LOAD COND.
CoorsTek PlasmaPure-UC™ 99.9% Alumina
Maximum Service Temperature, Air 1750 °C
3180 °F
limited
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite
Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum..
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
China-Yixing Longly Refractories Push Slab Corundum-Mullite
Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine..
Maximum Service Temperature, Air 1750 °C
3180 °F
limited
Chosun Refractories TPA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1750 °C
3180 °F
Anderman Ceramics EA995 Sintered Alumina, 99.5%
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
Maximum Service Temperature, Air 1750 °C
3180 °F
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast LP 100 Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual..
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast LP 85 KP Dense Refractory Brick
Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl..
Maximum Service Temperature, Air 1750 °C
3180 °F
Gouda Vuurvast LP 85 KP Dense Refractory Brick
Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl..
Maximum Service Temperature, Air 1750 °C
3180 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast LP 97-3 Dense Refractory Brick
Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can ..