Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURAS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in good slag resistance and high strength properties at lower temperatures. The mechanical strength of this product is developed after heating above 150°C.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 1.35 - 1.55 W/m-K

@Temperature 100 °C
9.37 - 10.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.40 - 1.60 W/m-K

@Temperature 600 °C
9.72 - 11.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.53 - 1.73 W/m-K

@Temperature 1600 °C
10.6 - 12.0 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 1750 °C
3180 °F
Shrinkage -1.50 - 0.500 %

@Temperature 1600 °C
-1.50 - 0.500 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 96 %
96 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 2.0 %
2.0 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2850 kg
Segercone 41