Physical Properties Metric English Comments
Bulk Density 3.83 g/cc
0.138 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength 345 MPa
50000 psi
205 MPa

@Temperature 538 °C
29700 psi

@Temperature 1000 °F
Compressive Strength 2550 MPa
370000 psi
Thermal Properties Metric English Comments
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 1000 °C
4.67 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 29.0 W/m-K
201 BTU-in/hr-ft²-°F
7.20 W/m-K

@Temperature 800 °C
50.0 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1750 °C
3180 °F
no load
Component Elements Properties Metric English Comments
Al2O3 99 %
99 %
CaO 0.030 %
0.030 %
Fe2O3 0.070 %
0.070 %
MgO 0.070 %
0.070 %
Na2O 0.050 %
0.050 %
SiO2 0.70 %
0.70 %