Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 85-10 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 90-5 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 90-8 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. The 8% chromium-oxide addition gives good volume stability at very high temperatures. Applications: chemical incinerators, combusti.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 70 M Dense Refractory Brick Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 80 FM Dense Refractory Brick Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 80 FM Dense Refractory Brick Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast CURON 170 GM Dense Refractory Castable Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 65 A Dense Refractory Brick Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics REFCAST LC80 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics REFCAST LC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Continuous |
Unifrax Fibermax® Duraboard® 17H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Continuous |
Unifrax Fibermax® Duraboard® 17R Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Continuous |
Zircar Ceramics AL-25/1700 Alumina Insulation AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | NO-LOAD COND. |
CoorsTek ADD-96 96% Alumina |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories HSC-85AL Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories MMCT-85 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories SFC-70 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Chosun Refractories 1700 HA BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Chosun Refractories CFA-2 Ceramic Foam Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast SiC 90 Dense Refractory Brick Description: Very good thermal shock resistance, abrasion resistance as well as very good heat conductivity makes this SiC based brick very well suited for muffles as well as for applications under .. |