Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1649 °C | 3000 °F | |
Pyrotek REDLINE MULTIKOTE Water-Based Coating A water-based coating designed to prevent molten metal adhesion to both refractory and most metallic surfaces. Multikote's bonding system enables it to be applied in a variety of applications .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURAS 85 P Moldable Refractory Material Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast LP 60 AAP Dense Refractory Brick Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Quick Immersion |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Sharadaa Ceramics PCF (AZS) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Quick Immersion |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Refractory Composites RS-99W Refractory Sheet Type RS-99W boards can be moistened with water and molded into any desired shape. After low temperature bake-out of 300°C (570°F) boards are unaffected by moisture.Information provided by ZIRCAR R.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics APA-1 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-1 is a strong, flexible material with fibers held together with organic binder that is available in roll or sheet.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories LPCT-16DS Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories PMCT-165 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories TCH-175S Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
BNZ Materials Super Blakbond Mortar Super Blakbond is an air-setting mortar for general purpose plant use. It has greater air-setting strength than Blakbond or No. 2986. It is good for insulating fire brick where greater bond strength.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Anderman Ceramics EA95 Sintered Alumina, 95% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia Castable ceramic with high dielectric and physical strength. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabind™ 643-1 High Temperature Inorganic Binder A basic solution compatible with most ceramic and metal powders. Excellent binder for producing high temperature protective coatings and refractory and chemically resistant adhesives and patching ma.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics AL-R/H Alumina Rigidizer/Hardener Type AL-R/H Alumina Rigidizer/Hardener is a single part water based colloidal suspension of alumina hydrate. Mainly used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic product.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |