Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 85.0 °C | 185 °F | UL-746 ABC |
Plaskolite Optix® CA - 51 KC General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | UL-746 ABC |
Plaskolite West Optix® CA - 51 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Recommended |
Nye Lubricants 759X (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 20,000 hr; IEC 216 |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; 5,000 h |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-SHIELD® 2003 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-SHIELD® 4904 Conductive Coating Conductive Nickel-Filled Acrylic Coating. This is the lowest coast in the family of nickel-filled, electrically conductive acrylic coatings. CHO-SHIELD® 4904 is resistant to solvent attack and to f.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | UL-746 ABC |
Plaskolite West Optix® CA - 51 KC General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 20,000 hr; IEC 216 |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 20,000 hr; IEC 216 |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 EO Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, lubricated in surface.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | RTI |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Maximum Service Temperature, Air | 85.0 - 140 °C | 185 - 284 °F | Average value: 109 °C Grade Count:7 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Fujipoly Industries FG-S Fine Connector Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Heat Distortion Temp |
Hannam Chemical Hanalac 711 ABS, Plating Grade Plating grade with excellent moldability and easy to surface treat. It also has a strong adhesive strength after plating and an excellent heat cycle. Applications: Appliances, TV frames, automoti.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Heat Distortion Temp |
Hannam Chemical Hanalac 780 ABS, High Flow FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Styrolution Luran® S 777 K UV Black 56625 ASA Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Styrolution Terluran® HH-106 Q109 Colored ABS Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R431 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R496 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R583 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R698 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R798 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 5000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM Epinyl PA 6 Polyamide 6 Characteristics: medium viscosity, good mechanical properties |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | long term |
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM) Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over .. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 5000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM PA 6 Polyamide 6 Characteristics: medium viscosity, general purpose |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous |
3M 9086 High Performance Double Coated Tapes with Adhesive 375 3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low s.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Long Term |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |