Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 115 - 260 °C | 239 - 500 °F | Average value: 249 °C Grade Count:20 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Maximum Service Temperature, Air | 220 - 260 °C | 428 - 500 °F | Average value: 248 °C Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Maximum Service Temperature, Air | 250 - 260 °C | 482 - 500 °F | Average value: 257 °C Grade Count:7 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Maximum Service Temperature, Air | 250 - 260 °C | 482 - 500 °F | Average value: 258 °C Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Maximum Service Temperature, Air | 25.0 - 260 °C | 77.0 - 500 °F | Average value: 136 °C Grade Count:61 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Maximum Service Temperature, Air | 250 - 260 °C | 482 - 500 °F | |
Zeus PEEK Tubing PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used.. |
|||
Maximum Service Temperature, Air | 250 - 260 °C | 482 - 500 °F | Average value: 257 °C Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Maximum Service Temperature, Air | 200 - 260 °C | 392 - 500 °F | Average value: 227 °C Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Maximum Service Temperature, Air | 180 - 260 °C | 356 - 500 °F | Average value: 215 °C Grade Count:25 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |