Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL-746 ABC |
Plaskolite Optix® CP - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Short Term |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL-746 ABC |
Plaskolite West Optix® CP - 80 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JLK51A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Dynamic |
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 EO Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding, with surface lubrication.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 W Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 90.0 - 250 °C | 194 - 482 °F | Average value: 164 °C Grade Count:23 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
LATI Latimass 62-07 D025 PA6, Impact Modified Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 65007 Polyvinyl Chloride, Flexible Notes: 90°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 02-A0310A-107 Polyvinyl Chloride, Semi-Rigid Notes: 80°C Insulation; RoHS Compliant Uses: Automotive Electronics; InsulationWire Types: GPTAgency Ratings: SAE J1128 Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor .. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 84856 Polyvinyl Chloride, Flexible Notes: 90°C Insulation; RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Cable JacketingAgency Ratings: UL 62; UL QMTT2 .E73402 Forms: Pellets Wire Types: SJTW; STWI.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Trelleborg B800 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous Use |
Polyram PlusTek PB500 Nylon 6, Flame Retardant Flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Trelleborg Emerson & Cuming Eccobond® 15 Clear Variable Hardness Catalyst Emerson & Cuming 15 Clear Eccobond® Variable Hardness CatalystEasy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. Long working life. Yields .. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | long term |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
3M 730 Clear Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
ATG s.r.l. SBR Styrene-Butadiene Rubber |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL-746 ABC |
Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Maximum Service Temperature, Air | 90.0 - 105 °C | 194 - 221 °F | |
Sylvin Technologies 6134-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Recommended continuous use |
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |