Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Continuous Use |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Continuous Use |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Acrylic |
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 129 °C Grade Count:18 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
LATI Latan 13E71 POM Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Pressed Bushings |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
Trelleborg Emerson & Cuming Stycast® 1265 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Dry Service |
Chesterton ARC 797 Low-viscosity, 100% solids, epoxy-based, concrete primer sealer Description: Its unique hydrophobic properties allow ARC 797 to be applied to damp concrete with excellent penetrating properties. When applied, ARC 797 will improve adhesion of subsequent topcoats .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Deflection Temp at unknown load |
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy AboCast 8503-4/AboCure 8503-4 is a general purpose, moderate speed, colorless epoxy casting compound with low viscosity. It offers a convenient 2/1 ratio by volume and lends itself to casting of thi.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long term |
3M 415 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long term |
3M 9420 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short term |
3M 9925XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long Term |
3M XG2105 Hi-Performance Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long Term |
3M XG5110 General Purpose Double Coated Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short Term |
3M XT2105-AGT Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short Term |
3M XT2112 Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short Term |
3M XT2112-AGT Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short term |
3M 415 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
GEHR Plastics ECOGEHR® C-L Cellulose-Lignin Compound
(discontinued **) C-L is comprised of the wood components cellulose, natural fibers, lignin and fatty acids. It possesses many interesting properties that together are very similar to the natural wood. Consequently,.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
BP Amoco Amoco® 7635 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR .. |
|||
Maximum Service Temperature, Air | 65.0 - 140 °C | 149 - 284 °F | Average value: 104 °C Grade Count:7 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 115 °C Grade Count:5 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Maximum Service Temperature, Air | 65.0 - 140 °C | 149 - 284 °F | Average value: 113 °C Grade Count:3 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |