3M XT2112-AGT Hi-Tack Adhesive Transfer Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M XT2112-AGT Hi-Tack Adhesive Transfer Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range of adhesive transfer and double- coated tapes designed for attachment of paper, corrugated, films, foils, fabric, plastics and metal. Double Coated (DC) tapes provide a backing for improved handling. Adhesive Transfer Tapes (ATT) provide the thinnest bond lines. The 3M X-Series Tape System is manufactured in the United States by 3M.Information provided by 3M
Physical Properties Metric English Comments
Thickness 81.3 microns
3.20 mil
Release Liner
127 microns
5.00 mil
Tape
Mechanical Properties Metric English Comments
Peel Strength 1.71 kN/m
9.75 pli
Stainless Steel, 180° Peel, 2 mil Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.0 °C
149 °F
Short Term
93.0 °C
199 °F
Long Term
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Adhesive Type High Tack Acrylic
Liner White Densified Kraft Liner with Red Print