Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1750 °C | 3180 °F | no load |
McDanel Advanced Ceramics AP 35 99% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 80-5 Dense Refractory Brick Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 98 Dense Refractory Brick Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette.. |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 99 S Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
ICE Al2O3 99.8 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Gouda Vuurvast AK 85 KM Dense Refractory Brick Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a.. |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 99 Dense Refractory Brick Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Gouda Vuurvast CURAS PBK Moldable Refractory Material Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Sharadaa Ceramics PHOSTCAST 90 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Sharadaa Ceramics REFCAST LC90ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | No Load |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | NO-LOAD COND. |
CoorsTek AD-996 99.6% Alumina |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | No Load |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | No Load |
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | NO-LOAD COND. |
CoorsTek PlasmaPure-UC™ 99.9% Alumina |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | limited |
Chosun Refractories BLC Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | limited |
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | limited |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | |
China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | |
China-Yixing Longly Refractories Push Slab Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | |
China-Yixing Longly Refractories Seggar Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Maximum Service Temperature, Air | >= 1750 °C | >= 3180 °F | |
China-Yixing Longly Refractories Shelf Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | limited |
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Maximum Service Temperature, Air | 1750 °C | 3180 °F | |
Gouda Vuurvast LP 85 KP Dense Refractory Brick Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl.. |