Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 80 B Dense Refractory Brick Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast AK 80 B Dense Refractory Brick Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast AK 82 A Dense Refractory Brick Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast LP 85 AM Dense Refractory Brick Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast LP 85 M Dense Refractory Brick Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs... |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 86 A Dense Refractory Brick Description: This bauxite based brick has a high strength and good erosion resistance. Application in torpedo ladles for the steel industry and outlet zone rotary cement kilns.Remarks: This data rep.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast AK 86 A Dense Refractory Brick Description: This bauxite based brick has a high strength and good erosion resistance. Application in torpedo ladles for the steel industry and outlet zone rotary cement kilns.Remarks: This data rep.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics 29 Insulation Bricks-ASTM Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Continuous |
Sharadaa Ceramics Heat Shield Zircon Rich Refractory Coating Characteristics: Easy to mix with water – User friendly; Easy to apply by toweling, brushing or spraying; Adequate dry strength; Good adhesion to metals, refractory bricks and castables; No sur.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics PCF60-1 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics PCF60-2 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics PCF70 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics REFCAST LC45 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Sharadaa Ceramics ZAP 008 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Continuous |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Safe Operating Temp |
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3 Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | limited |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Intermittent |
Zircar Ceramics ALCAA Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Continuous |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | Continuous |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |
|||
Maximum Service Temperature, Air | 1550 °C | 2820 °F | |
Gouda Vuurvast SiC 70 Dense Refractory Brick Description: This type of brick, based on silicon carbide, is because of a very good thermal shock resistance, abrasion resistance and a high thermal conductivity very well suited for waste incinera.. |