Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast GOLITE 155 Refractory Insulating Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name GOLITE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast GOLITE 155 Refractory Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 15.0 - 21.0 MPa

@Temperature 100 °C
2180 - 3050 psi

@Temperature 212 °F
Cold Crushing Strength
22.0 - 28.0 MPa

@Temperature 1370 °C
3190 - 4060 psi

@Temperature 2500 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.360 - 0.460 W/m-K

@Temperature 100 °C
2.50 - 3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.410 - 0.510 W/m-K

@Temperature 600 °C
2.85 - 3.54 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.470 - 0.570 W/m-K

@Temperature 1370 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Maximum Service Temperature, Air 1550 °C
2820 °F
Shrinkage -0.600 - 0.600 %

@Temperature 1370 °C
-0.600 - 0.600 %

@Temperature 2500 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 52 %
52 %
SiO2 38 %
38 %
Descriptive Properties Value Comments
ASTM Classification S
Material Consumption per 1 m3 1430 kg
Mixing Water 20-25 liters
per 100 kgs dry material