Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit AS Phenolic, Paper Reinforcement, Black, Sheets
Description: ESD-protection quality according to SP-method 2472, IEC 61340-5-1 and EN 100015-1. SP ESD Approval Certificate No. 230-01-0137. High mechanical properties at temperatures up to 120°CAp..
Maximum Service Temperature, Inert 120 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola Etronit B 65 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Good electrical properties at normal air humidity.Applications: Winding tubes in the foil and metal foil industries and carrier t..
Maximum Service Temperature, Inert 120 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola Etronit B 66 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: Specially designed for high-voltage insulation with high requirements for insulating capacity along the tube.Applications: Insulating tubes in high-voltage switchgear and tap changers....
Maximum Service Temperature, Inert 120 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola Etronit B67 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Very good electrical properties at high air humidity. Applications: Winding tubes in the foil and metal foil industries and carri..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit I Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity.Application: Insulation material in hig..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected and lasting electrical properties despit..
Maximum Service Temperature, Inert 120 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Tubes
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig..
Maximum Service Temperature, Inert 120 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola Etronit IV C S Phenolic, Paper Reinforcement, Black, Tubes
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr..
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha..
Copyright © lookpolymers.com All Rights Reserved