Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets

Category Polymer , Thermoset , Phenolic
Manufacturer Elektro-Isola
Trade Name Etronit
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected and lasting electrical properties despite the impact of moisture. Suitable as high-frequency insulation on account of the very low dielectric loss factor. Very low water absorption.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Water Absorption 0.80 %
0.80 %
24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2
Mechanical Properties Metric English Comments
Tensile Strength 90.0 MPa

@Thickness >=1.50 mm
13100 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Modulus of Elasticity 7.00 GPa

@Thickness >=1.50 mm
1020 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Flexural Strength 130 MPa

@Thickness >=1.50 mm
18900 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Thickness >=5.00 mm
1.43 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+8 ohm

@Thickness >=3.00 mm
1.00e+8 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Dielectric Constant 5.0

@Thickness <=3.00 mm,
Frequency 50.0 Hz
5.0

@Thickness <=0.118 in,
Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2
5.0

@Thickness <=3.00 mm,
Frequency 1.00e+6 Hz
5.0

@Thickness <=0.118 in,
Frequency 1.00e+6 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2
Dielectric Strength 1.20 kV/mm

@Thickness >=3.00 mm
30.5 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
8.50 kV/mm

@Thickness 3.00 mm
216 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Dissipation Factor 0.025

@Frequency 50.0 Hz
0.025

@Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2
0.025

@Frequency 1.00e+6 Hz
0.025

@Frequency 1.00e+6 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2
Comparative Tracking Index 100 V

@Thickness 3.00 mm
100 V

@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4