| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 | 
| Water Absorption | 1.47 % | 1.47 % | 24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength |           110           MPa           @Thickness >=1.50 mm  | 
                  16000           psi           @Thickness >=0.0591 in  | 
        24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 | 
| Modulus of Elasticity |           8.00           GPa           @Thickness >=1.50 mm  | 
                  1160           ksi           @Thickness >=0.0591 in  | 
        24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 | 
| Flexural Strength |           160           MPa           @Thickness >=1.50 mm  | 
                  23200           psi           @Thickness >=0.0591 in  | 
        24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1 | 
| Compressive Strength |           300           MPa           @Thickness >=5.00 mm  | 
                  43500           psi           @Thickness >=0.197 in  | 
        24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 | 
| Shear Strength |           35.0           MPa           @Thickness >=5.00 mm  | 
                  5080           psi           @Thickness >=0.197 in  | 
        24hr/23°C/50% RH; IEC/EN 60893-2 5.5 | 
| Izod Impact, Notched (ISO) |           3.30           kJ/m²           @Thickness >=5.00 mm  | 
                  1.57           ft-lb/in²           @Thickness >=0.197 in  | 
        24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Maximum Service Temperature, Inert |           120           °C           @Thickness 0.000 mm, Time 7.20e+7 sec  | 
                  248           °F           @Thickness 0.000 in, Time 20000 hour  | 
        IEC 60216; IEC/EN 60893-2 7.1 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Insulation Resistance |           1.00e+8           ohm           @Thickness >=3.00 mm  | 
                  1.00e+8           ohm           @Thickness >=0.118 in  | 
        24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 | 
| Dielectric Constant |           5.0                     @Thickness <=3.00 mm, Frequency 50.0 Hz  | 
                  5.0                     @Thickness <=0.118 in, Frequency 50.0 Hz  | 
        96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2 | 
| Dielectric Strength |           1.20           kV/mm           @Thickness >=3.00 mm  | 
                  30.5           kV/in           @Thickness >=0.118 in  | 
        24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 | 
|           10.0           kV/mm           @Thickness 3.00 mm  | 
                  254           kV/in           @Thickness 0.118 in  | 
        24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 | |
| Dissipation Factor |           0.040                     @Frequency 50.0 Hz  | 
                  0.040                     @Frequency 50.0 Hz  | 
        96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2 | 
| Comparative Tracking Index |           100           V           @Thickness 3.00 mm  | 
                  100           V           @Thickness 0.118 in  | 