Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.190 - 0.220 W/m-K | 1.32 - 1.53 BTU-in/hr-ft²-°F | Average value: 0.202 W/m-K Grade Count:5 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Thermal Conductivity | 0.190 - 0.220 W/m-K | 1.32 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Thermal Conductivity | 0.190 - 0.220 W/m-K | 1.32 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Thermal Conductivity | 0.135 - 0.220 W/m-K | 0.937 - 1.53 BTU-in/hr-ft²-°F | Average value: 0.195 W/m-K Grade Count:12 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.190 - 0.220 W/m-K | 1.32 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Thermal Conductivity | 0.200 - 0.220 W/m-K | 1.39 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON M-300H PCTFE Granular Molding Powder NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by.. |
|||
Thermal Conductivity | 0.200 - 0.220 W/m-K | 1.39 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON M-300P PCTFE Pellets NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries. |
|||
Thermal Conductivity | 0.200 - 0.220 W/m-K | 1.39 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON M-400H PCTFE Granular Molding Powder NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process.. |
|||
Thermal Conductivity | 0.190 - 0.220 W/m-K | 1.32 - 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Thermal Conductivity | 0.202 - 0.220 W/m-K | 1.40 - 1.53 BTU-in/hr-ft²-°F | Average value: 0.210 W/m-K Grade Count:5 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Thermal Conductivity | 0.190 - 0.220 W/m-K | 1.32 - 1.53 BTU-in/hr-ft²-°F | Average value: 0.205 W/m-K Grade Count:11 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |