Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.20 - 1.50 W/m-K | 8.33 - 10.4 BTU-in/hr-ft²-°F | |
Parker Chomerics CHO-BOND 584-208 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics THERM-A-FORM T642 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-Fk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-Hk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott DURAN® Borosilicate Glass Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, general-purpose glass for apparatus for the chemical industry, for pipelines, and glasswareInformation provided by.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott DUROBAX® amber Neutral Glass Tubing Neutral glass tubing, chemically highly resistant, with light protection Containers, test tubes, pipettes, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, .. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8250 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8270 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8347 Borosilicate Glass Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, highly UV-transmitting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium i.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8487 Borosilicate Glass Borosilicate glass for sealing to tungsten Backlights, flash lamps, lamp bulbs, exhaust and flare bulbs The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is .. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8687 Borosilicate Glass Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8688 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8689 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® B912-8 Epoxy Product Description: A single component, thermally and electrically conductive, epoxy adhesive designed for semiconductor die attach and circuit assembly applications. Its unique features are a pot.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® EM127 Electrically Conductive Epoxy Product Description: EPO-TEK® EM127 is a single component, heat curable, electrically conductive epoxy adhesive for semiconductor IC and LED die attach applications.Advantages & Application Notes: .. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |
|||
Thermal Conductivity | >= 1.20 W/m-K | >= 8.33 BTU-in/hr-ft²-°F | |
Arlon 0.008" (0.2032 mm) Thermabond®-45 Uncured Silicone (99720W008) 0.008 in., +0.000,-0.002(0.2 mm, +0.00, -0.05) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in +0.000,-0.002(0... |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C). |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott CONTURAX® Borosilicate Glass Borosilicate glass tubing and rod, varying types of inner and outer shapes Lighting, giftware, and decoration The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |