Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.00 - 3.50 W/m-K | 20.8 - 24.3 BTU-in/hr-ft²-°F | Through Plane; ASTM E1461 |
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Thermal Conductivity | 3.00 W/m-K | 20.8 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Thermal Conductivity | 3.00 W/m-K | 20.8 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl.. |
|||
Thermal Conductivity | 3.00 W/m-K | 20.8 BTU-in/hr-ft²-°F | Silicone property; ASTM E1530 |
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive
(discontinued **) Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas |
|||
Thermal Conductivity | 3.00 W/m-K | 20.8 BTU-in/hr-ft²-°F | |
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
Thermal Conductivity | 3.00 W/m-K | 20.8 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Thermal Conductivity | 2.99 W/m-K | 20.8 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Thermal Conductivity | 3.00 W/m-K @Temperature 100 °C |
20.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E 1530 |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Thermal Conductivity | 3.00 W/m-K | 20.8 BTU-in/hr-ft²-°F | Silicone Property; ASTM E 1530 |
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive
(discontinued **) Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer. |