Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.263 W/m-K | 1.83 BTU-in/hr-ft²-°F | |
Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED). |
|||
Thermal Conductivity | 0.263 W/m-K | 1.83 BTU-in/hr-ft²-°F | |
Arlon IsoClad 933 Non-Woven Fiberglass Reinforced PTFE Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED). |
|||
Thermal Conductivity | 0.264 W/m-K | 1.83 BTU-in/hr-ft²-°F | Melt |
BASF Ultramid® 8202 HS PA6 (Conditioned) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Thermal Conductivity | 0.264 W/m-K | 1.83 BTU-in/hr-ft²-°F | Melt |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Thermal Conductivity | 0.264 W/m-K | 1.83 BTU-in/hr-ft²-°F | Melt |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Thermal Conductivity | 0.264 W/m-K | 1.83 BTU-in/hr-ft²-°F | Melt |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |