Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.0 W/m-K @Temperature 100 °C |
111 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | RT |
Outokumpu 4742 High Temperature Ferritic Stainless Steel Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 100 °C |
111 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 100 °C |
111 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | |
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
Thermal Conductivity | >= 16.0 W/m-K | >= 111 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Therma-Tech™ NJC-6500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 20.0 °C |
111 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Mateck Laser Grade Zinc Selenide, ZnSe CVD Optical Crystals |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | |
Goodfellow Chromaloy O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | |
Goodfellow Aluchrom O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Thermal Conductivity | 16.0 - 20.0 W/m-K | 111 - 139 BTU-in/hr-ft²-°F | in parallel (002) direction |
Momentive Performance Materials HOPG Graphite Monochromator Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | |
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | |
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 100 °C |
111 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | |
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |