Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Poco Graphite PLS Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Strip; 1/2H (TD02) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5Formability Ratio (bad Way): 1Superficial Hardness: 30T 74-79Tabulated properties appl.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 74%Superficial Hardness: 30N 58-6.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium Formall® 545 Aluminum Alloy Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Poco Graphite TM Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |