Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 (dry sample) |
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 (dry sample) |
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data) Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp.. |
|||
Thermal Conductivity | 0.280 - 1.10 W/m-K | 1.94 - 7.63 BTU-in/hr-ft²-°F | Average value: 0.553 W/m-K Grade Count:3 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PA 6.6 Nylon 6.6, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2212 PEI (Europe-Africa-Middle East) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6.6 FG Polyamide 6.6, Food Grade This material has good hardness, wear resistance, abrasion strength and impact strength.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6.6 Polyamide 6.6 This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL.. |