Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 141R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 241 PC General Purpose polycarbonate with 10.5 of melt flow rate. Improved flame retardance. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 141 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 141R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic 1120 Corrosion-Resistant Panels Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | |
Trelleborg Offshore Vikotherm™ 73785 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® 1269A Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 125 PTFE, 35% Carbon Filled Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | Melt; DIN 52612 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic GLASTHERM HT Insulation Sheet Glastherm Grade HT is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT is completely as.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |