Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.155 W/m-K | 1.08 BTU-in/hr-ft²-°F | Melt |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Thermal Conductivity | 0.155 W/m-K | 1.08 BTU-in/hr-ft²-°F | Melt |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (DAM) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Thermal Conductivity | 0.155 W/m-K | 1.08 BTU-in/hr-ft²-°F | |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 100 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt.. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |