Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™ VORACTIV™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalytic activity make it well suited for high-resilience, flexible molded foams. These foams may be made utilizing TDI, TDI/MDI blends, or all-MDI isocyanate compositions.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Density 1.02 g/cc
0.0368 lb/in³
Viscosity Measure 600 - 700 cSt

@Temperature 37.8 °C
600 - 700 cSt

@Temperature 100 °F
Maximum Moisture Content 0.080
0.080
Vapor Pressure <= 0.000133 bar
<= 0.100 torr
ASTM Color <= 75
<= 75
APHA
Thermal Properties Metric English Comments
Specific Heat Capacity 1.84 J/g-°C

@Temperature 20.0 °C
0.440 BTU/lb-°F

@Temperature 68.0 °F
2.00 J/g-°C

@Temperature 60.0 °C
0.478 BTU/lb-°F

@Temperature 140 °F
2.09 J/g-°C

@Temperature 100 °C
0.500 BTU/lb-°F

@Temperature 212 °F
Thermal Conductivity 0.163 W/m-K
1.13 BTU-in/hr-ft²-°F
0.155 W/m-K

@Temperature 100 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.159 W/m-K

@Temperature 50.0 °C
1.10 BTU-in/hr-ft²-°F

@Temperature 122 °F
Flash Point >= 204 °C
>= 399 °F
PMCC
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 30 - 34