Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 26.0 - 120 µm/m-°C | 14.4 - 66.7 µin/in-°F | Average value: 85.4 µm/m-°C Grade Count:71 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 100 - 120 µm/m-°C @Temperature 20.0 °C |
55.6 - 66.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
CTE, linear | 108 - 120 µm/m-°C | 60.0 - 66.7 µin/in-°F | Average value: 116 µm/m-°C Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
CTE, linear | 120 - 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 - 66.7 µin/in-°F @Temperature 212 - 392 °F |
Average value: 120 µm/m-°C Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 90.0 - 120 µm/m-°C | 50.0 - 66.7 µin/in-°F | ASTM D696 |
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon® |
|||
CTE, linear | 100 - 120 µm/m-°C | 55.6 - 66.7 µin/in-°F | ASTM D696 |
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel PTFE G Special Compound with steelInformation provided by Guarniflon® |
|||
CTE, linear | 90.0 - 120 µm/m-°C | 50.0 - 66.7 µin/in-°F | ASTM D696 |
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon® |
|||
CTE, linear | 110 - 120 µm/m-°C | 61.1 - 66.7 µin/in-°F | ASTM D696 |
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne.. |
|||
CTE, linear | 100 - 120 µm/m-°C | 55.6 - 66.7 µin/in-°F | ASTM D696 |
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high .. |
|||
CTE, linear | 100 - 120 µm/m-°C @Temperature 20.0 °C |
55.6 - 66.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
CTE, linear | 85.0 - 120 µm/m-°C | 47.2 - 66.7 µin/in-°F | Average value: 96.4 µm/m-°C Grade Count:14 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 43.2 - 120 µm/m-°C | 24.0 - 66.7 µin/in-°F | Average value: 83.3 µm/m-°C Grade Count:27 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 90.0 - 120 µm/m-°C | 50.0 - 66.7 µin/in-°F | Average value: 98.4 µm/m-°C Grade Count:8 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 31.0 - 120 µm/m-°C | 17.2 - 66.7 µin/in-°F | Average value: 69.8 µm/m-°C Grade Count:10 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 120 - 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 - 66.7 µin/in-°F @Temperature 212 - 392 °F |
Average value: 120 µm/m-°C Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
CTE, linear | 30.0 - 120 µm/m-°C | 16.7 - 66.7 µin/in-°F | Average value: 68.9 µm/m-°C Grade Count:127 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |