Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific) |
|||
CTE, linear | 40.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
CTE, linear | 20.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.1 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® LCG0820 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 2.00 - 50.0 µm/m-°C | 1.11 - 27.8 µin/in-°F | Average value: 23.8 µm/m-°C Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
CTE, linear | 22.0 - 50.0 µm/m-°C | 12.2 - 27.8 µin/in-°F | Average value: 36.0 µm/m-°C Grade Count:3 |
Overview of materials for Polystyrene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear | 12.0 - 50.0 µm/m-°C | 6.67 - 27.8 µin/in-°F | Average value: 28.7 µm/m-°C Grade Count:33 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
CTE, linear | 10.0 - 50.0 µm/m-°C | 5.56 - 27.8 µin/in-°F | Average value: 25.9 µm/m-°C Grade Count:27 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
CTE, linear | 35.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL S100G10 PPE+PS (Asia Pacific) |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX CRN530 PPE+PA6 (Asia Pacific) 30%GF GTX grade for Non Auto market |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Noryl GTX GTX880 PPE+PA6 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX GTX6801 PPE+PA (Asia Pacific) PPE+PA, GF 30% |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 45.0 - 50.0 µm/m-°C | 25.0 - 27.8 µin/in-°F | |
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi.. |
|||
CTE, linear | 40.0 - 50.0 µm/m-°C | 22.2 - 27.8 µin/in-°F | |
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |
|||
CTE, linear | 45.0 - 50.0 µm/m-°C | 25.0 - 27.8 µin/in-°F | |
Master Bond UV10TKMed One component UV curable, biocompatible, high viscosity compound Product Description: Master Bond UV10TKMed is a higher viscosity, one part UV system for bonding, sealing and coating that passes USP Class VI testing along with ISO 10993-5 for cytotoxicity. It has.. |
|||
CTE, linear | 45.0 - 50.0 µm/m-°C | 25.0 - 27.8 µin/in-°F | |
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi.. |
|||
CTE, linear | 45.0 - 50.0 µm/m-°C | 25.0 - 27.8 µin/in-°F | |
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper.. |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-16 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 36.0 - 50.0 µm/m-°C | 20.0 - 27.8 µin/in-°F | Average value: 43.2 µm/m-°C Grade Count:5 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
CTE, linear | 0.702 - 50.0 µm/m-°C | 0.390 - 27.8 µin/in-°F | Average value: 29.7 µm/m-°C Grade Count:7 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
CTE, linear | 20.0 - 50.0 µm/m-°C | 11.1 - 27.8 µin/in-°F | Average value: 32.5 µm/m-°C Grade Count:19 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |